What Is Cast Iron
Cast iron is a family of iron-carbon alloys containing more than 2% carbon. The main types of cast iron are gray iron, ductile iron, white iron, malleable iron and compacted graphite iron (CGI). Alloy cast irons are also used when additional wear, heat or corrosion resistance is required.
The main difference between these cast iron types comes from their graphite shape, matrix structure and alloying elements. These differences directly affect tensile strength, hardness, elongation, machinability, wear resistance and applications.
In this guide, we compare the major cast iron materials and grades to help you choose the right material for industrial castings.
Cast Iron Types and Properties Comparison
| Cast Iron Type | Structure | Strength | Hardness | Elongation | Key Property | Typical Applications |
|---|---|---|---|---|---|---|
| Gray Cast Iron | Flake graphite | Medium | Medium | Very Low | Excellent damping and machinability | Machine bases, housings, brake drums |
| Ductile Cast Iron | Spheroidal graphite | High | Medium | High | Strength and toughness | Valves, pipes, gears, heavy machinery |
| White Cast Iron | Carbide-rich structure | High / Brittle | Very High | Very Low | Excellent abrasion resistance | Crusher liners, mill liners, pump wear parts |
| Malleable Cast Iron | Temper carbon | Medium | Medium | Medium | Toughness and machinability | Pipe fittings, brackets, hardware |
| Compacted Graphite Iron | Compacted graphite | High | Medium | Low–Medium | Strength + thermal performance | Engine blocks, cylinder heads |
| Alloy Cast Iron | Grade-dependent | Varies | Varies | Varies | Wear, heat or corrosion resistance | Mining, pumps, chemical equipment |
Common Cast Iron Grades and Standards
| Cast Iron Material | Common ASTM Standard | Typical Grades / Classes |
|---|---|---|
| Gray Cast Iron | ASTM A48/A48M | Class 20, 25, 30, 35, 40 and higher |
| Ductile Cast Iron | ASTM A536 | 60-40-18, 65-45-12, 80-55-06, 100-70-03 |
| White / Abrasion-Resistant Cast Iron | ASTM A532/A532M | Multiple abrasion-resistant classes |
| Malleable Cast Iron | ASTM A47/A47M | Grade 32510 |
| Compacted Graphite Iron | ASTM A842 | CGI grades according to required properties |
How to Choose the Right Type of Cast Iron
Choosing the right type of cast iron depends on how the part will be used. Instead of comparing materials by strength alone, you should consider load, impact, wear, vibration, temperature, machinability, and the applicable material standard.
| If Your Part Requires | Consider | Why |
|---|---|---|
| Good vibration damping and machinability | Gray Cast Iron | Flake graphite provides excellent damping and generally good machinability |
| Higher strength and impact resistance | Ductile Cast Iron | Nodular graphite provides better toughness and ductility than gray iron |
| High abrasion and wear resistance | White or Alloy Cast Iron | Hard carbide-rich structures provide strong wear resistance |
| Small fittings and mechanical components | Malleable Cast Iron | Provides a useful combination of toughness and machinability |
| Higher strength with good thermal performance | Compacted Graphite Iron (CGI) | Offers a balance between strength, stiffness, and thermal performance |
Your final material choice should also consider the specific grade, section thickness, operating load, impact, temperature, corrosion environment, machining requirements, and applicable ASTM or other material standards.
The 6 Main Types of Cast Iron Explained
Gray Cast Iron
Chemical Composition of Gray Cast Iron
Carbon: 2%–4%
Silicon: 1.0%–2.0%
Manganese: 0.5%–1.4%
Phosphorus: 0.02%
Sulfur: 0.05%

Mechanical Properties of Gray Cast Iron
The graphite appears in flake form, reducing the effective load-bearing area, so gray cast iron has lower strength, ductility, and toughness than other cast irons.
The fracture surface appears dark gray when broken. It is easy to machine and has good wear resistance, but it is brittle.
It has the lowest cost and is the most widely used type of cast iron.
Mainly used for frames, housings, and similar components.
Applications of Gray Cast Iron
Because gray cast iron has good compressive strength, excellent vibration damping, good wear resistance, and is easy to machine, gray iron castings play an important role in machinery manufacturing. It is very suitable for machine tool beds such as lathes, milling machines, and grinding machines.

White Cast Iron
Chemical Composition of White Cast Iron
Carbon: 2.5%–4.3%
Silicon: 1%–3%
Manganese: 0.25%–1%
Sulfur: 0.1%–0.3%
Phosphorus: 0.05%–1%
Characteristics of White Cast Iron
White cast iron contains lower carbon and silicon; carbon mainly exists in the form of cementite, and the fracture surface is bright white.
It has large shrinkage during solidification and is prone to shrinkage cavities and cracks.
It has high hardness and high brittleness and cannot withstand impact loads.
It is mostly used as the base material for malleable cast iron and for producing wear-resistant parts.
Industrial Uses of White Cast Iron
White cast iron is easy to produce and low-cost. It is widely used for wear-resistant components and can also be used for small ball mills, slurry pump blades, liners, and crusher hammers that are subject to impact and wear.

Ductile Cast Iron (Nodular Iron)
Nodular Cast Iron Material Composition
Carbon: 3.0%–4.0%
Silicon: 1.8%–3.2%
The total content of manganese, phosphorus, and sulfur does not exceed 3.0%
Key Characteristics of Ductile Cast Iron
The graphite appears in spherical form. It is obtained by spheroidizing gray cast iron and is also called nodular iron.
It has higher strength and better toughness than gray cast iron.
Its properties can be adjusted through various heat treatments.
Mainly used for crankshafts, connecting rods, gears, clutch plates, hydraulic cylinder blocks, and other power machinery components.
Use Cases of Ductile Cast Iron
Ductile cast iron has excellent elongation and is commonly used for gears and bearings in mechanical parts, as well as engine blocks and cylinder heads in the automotive industry.

Malleable Cast Iron
Cast Iron Chemical Makeup
Carbon: 2.2%–2.8%
Silicon: 1.0%–1.8%
Sulfur: below 0.2%
Phosphorus: below 0.1%
Performance Characteristics of Malleable Cast Iron
The graphite appears in temper-carbon clusters, obtained by annealing white cast iron; it is also called tough iron.
It has uniform structure and good wear resistance.
Used to manufacture complex-shaped parts that can withstand strong dynamic loads.
Industrial Uses of Malleable Cast Iron
Malleable iron fittings have excellent wear resistance and are very suitable for industrial pipe elbows, tees, joints, unions, and bushings.

Compacted Graphite Iron (CGI)
CGI Alloy Composition
Carbon: 3.4%–3.6%
Silicon: 1.0%–1.8%
Manganese: 0.4%–0.6%
Sulfur: <0.06%
Phosphorus: <0.07%
Performance Characteristics of CGI
The graphite appears in worm-like form and is obtained by vermicularizing gray cast iron.
Higher strength than gray iron and lower toughness than ductile iron.
Mechanical properties are close to ductile cast iron.
Casting performance lies between gray iron and ductile iron.
Used to manufacture automotive components.
Applications of Compacted Graphite Iron
Compacted graphite iron combines the properties of ductile and gray cast iron. It is mainly used in automotive engines, exhaust manifolds, glass molds, diesel cylinder heads, and brake parts.

Alloy Cast Iron
Alloying Elements in Cast Iron
Carbon: 2.4%–4.0%
Silicon: 1%–3%
Manganese: 0.2%–1.2%
Phosphorus: 0.04%–1.2%
Nickel, chromium, molybdenum, and copper content exceeds 10%
Key Performance Characteristics of Alloy Cast Iron
By adding a certain amount of alloying elements to cast iron, it obtains special properties such as wear resistance, high-temperature resistance, and corrosion resistance. This type is called alloy cast iron.
Common alloy cast irons include wear-resistant cast iron, heat-resistant cast iron, and corrosion-resistant cast iron.
Mainly used for machine tool guideways, cylinder sleeves, and ball mill liners.
Applications & Industrial Use Cases of Alloy Cast Iron
Because alloy cast iron has excellent mechanical properties, it is widely used in engines, chemical equipment, pumps, and compressors. Due to its affordable price, it replaces cast steel and forged parts in many environments.
Cast Iron vs Cast Steel
Cast iron and cast steel are both widely used for industrial components, but their properties vary significantly by grade. The better choice depends on the required strength, toughness, wear resistance, machinability, casting complexity, and service conditions.
| Factor | Cast Iron | Cast Steel |
|---|---|---|
| Carbon Content | Generally higher | Generally lower |
| Castability | Generally good, especially for complex shapes | Usually requires tighter process control |
| Ductility & Toughness | Varies significantly by cast iron type | Generally higher |
| Vibration Damping | Particularly good in gray cast iron | Generally lower |
| Machinability | Highly grade-dependent | Highly grade-dependent |
| Typical Selection | Damping, wear resistance, castability, or cost-sensitive components | Toughness, impact resistance, and heavily loaded components |
Neither material is universally better. Your final choice should be based on the specific cast iron or steel grade, part geometry, mechanical requirements, operating conditions, and manufacturing process.
Common Applications of Different Cast Iron Types
Different cast iron grades are used in different industries depending on their mechanical properties and cost requirements.
- Gray Cast Iron: Machine tool bases, engine blocks, housings, brake drums.
- Ductile Cast Iron: Valves, pumps, pipes, gears, automotive components.
- White Cast Iron: Crusher liners, mill liners, slurry pump parts, wear plates.
- Malleable Cast Iron: Pipe fittings, brackets, hand tools, hardware components.
- Compacted Graphite Iron (CGI): Diesel engine blocks, cylinder heads, exhaust manifolds.
- Alloy Cast Iron: Mining equipment, chemical equipment, compressors, high-wear industrial parts.
For custom components made from gray iron, ductile iron, and other cast iron grades, explore our custom iron parts manufacturing capabilities.
Conclusion
Cast iron is a reliable material option for engineering projects. Its unique properties and functions make it widely used in the construction industry, automotive manufacturing, and household products.
MATSON METAL provides one-stop services for metal-related projects. If you are looking for high-quality cast iron materials, please contact us. With a wide variety of metals, extensive experience, and professional service, MATSON METAL can meet your needs.
FAQ
What Are the Four Main Types of Cast Iron?
The four traditional main types are gray cast iron, white cast iron, ductile cast iron, and malleable cast iron. Modern engineering classifications may also include compacted graphite iron and alloy cast iron depending on the application and classification system.
Which Type of Cast Iron Has the Best Wear Resistance?
White cast iron and high-alloy cast iron offer the highest wear resistance. White iron contains a hard cementite carbide network, while alloyed cast iron (with Cr/Mo/Ni) forms additional hard carbides that extend service life in abrasive applications such as crusher liners, pump housings, and mining components.
What Is the Difference Between Alloyed Cast Iron and Standard Cast Iron?
Alloyed cast iron contains additional elements such as chromium, nickel, and molybdenum. These alloying elements refine the microstructure, increase carbide formation, and significantly improve wear resistance, heat resistance, and corrosion performance. Standard cast iron does not offer the same durability in demanding environments.
Is Ductile Iron Stronger Than Gray Cast Iron?
Yes. Ductile iron provides significantly higher tensile strength, impact resistance, and elongation than gray cast iron because its graphite exists in spherical rather than flake form. It is commonly used for pressure-containing and load-bearing components.
Can Cast Iron Be Welded and Machined?
Most cast iron grades can be machined, although machinability varies by type. Gray cast iron is generally the easiest to machine. Welding is possible for some grades but usually requires preheating and controlled cooling to reduce the risk of cracking.
Related Resources: