🇺🇸English
Blog

Yield Strength of Aluminum: Common Alloys, Tempers & Material Selection

Aluminum does not have one universal yield strength. The value changes with alloy, temper, product form, heat treatment, and manufacturing process. If you are selecting aluminum for CNC machining, casting, forging, or another industrial part, specifying only “aluminum” is not enough.

For load-bearing components, yield strength matters because it indicates the stress at which permanent deformation begins.

What Is the Yield Strength of Aluminum?

Yield strength is the stress at which a material begins to deform permanently. Aluminum alloys commonly use the 0.2% offset yield strength to define this point.

Yield strength describes the start of permanent deformation. Tensile strength is the maximum stress a material can withstand before it breaks. For brackets, shafts, housings, and structural parts that must retain their shape, yield strength is usually the more relevant design value.

Yield Strength of Common Aluminum Alloys

The following values are typical engineering figures for general comparison. Final design values must be confirmed against the applicable material specification, product form, and supplier certificate.

AlloyTemperTypical Yield StrengthTypical Tensile StrengthCommon Use
5052H32About 193 MPaAbout 228 MPaSheet and formed parts
6063T5/T6About 145–214 MPaAbout 186–241 MPaExtrusions
6061T6About 276 MPaAbout 310 MPaCNC machined parts
2024T3About 290–345 MPaAbout 435–485 MPaHigh-strength components
7075T6About 503 MPaAbout 572 MPaHigh-strength lightweight parts
A356T6About 150–230 MPa*About 220–300 MPa*Cast aluminum parts

*A356-T6 properties vary with casting method, section thickness, internal quality, and heat treatment.

Why Does Aluminum Yield Strength Vary?

Alloy Composition

5xxx alloys use magnesium for corrosion resistance and formability. 6xxx alloys use magnesium and silicon for a balance of strength and machinability. 2xxx alloys use copper for higher strength, while 7xxx alloys use zinc and magnesium for very high strength.

Temper Condition

Common conditions include O (annealed), H (strain hardened), T4 (solution treated and naturally aged), T5 (artificially aged after cooling), T6 (solution treated and artificially aged), and T651 (T6 with stress relief). 6061 and 6061-T6 are therefore not a complete equivalent material requirement. Drawings should specify both alloy and temper.

Aluminum Density and Strength-to-Weight Ratio

Most common aluminum alloys have a density of about 2.7 g/cm³, roughly one-third the density of steel. Aluminum may not exceed steel in absolute strength, but it can offer a useful strength-to-weight ratio for aerospace parts, robotics, automation equipment, sports components, and lightweight structures.

Cast and CNC machined aluminum parts inspected on a factory workbench

Wrought vs. Cast Aluminum Yield Strength

Wrought Aluminum

6061, 7075, 2024, and 5052 are common wrought alloys used for plate, bar, extrusion, forging, and CNC machining. When product form and temper are specified, their properties are generally easier to control against the relevant material standard.

Cast Aluminum

A356 and similar cast alloys suit complex, near-net-shape components. Porosity, shrinkage, section thickness, solidification conditions, heat treatment, and internal quality can all affect the final result. Do not use 7075-T6 plate data to judge whether an A356 casting meets a design requirement.

How to Select Aluminum for CNC Machining

RequirementStarting Option
General CNC machining6061-T6
Higher strength-to-weight ratio7075-T6
High-strength machined parts2024-T3
Formability and corrosion resistance5052-H32
Extruded profiles6063-T5/T6
Complex cast componentsA356-T6

Also consider machinability, corrosion resistance, dimensional stability, finishing compatibility, cost, quantity, and critical tolerances.

Common Aluminum Strength-Specification Mistakes

  • Writing “aluminum” without an alloy and temper.
  • Using tensile strength in place of yield strength.
  • Applying wrought-alloy data directly to a casting.
  • Choosing the strongest alloy without considering corrosion, machinability, finishing, and cost.

How Should You Choose the Right Aluminum Alloy?

Start with the part’s load, geometry, weight target, environment, process, surface treatment, tolerances, quantity, and total manufacturing cost. 6061-T6 is often a balanced starting point for CNC machining. 7075-T6 suits higher strength-to-weight requirements. 2024-T3 targets high-strength machined parts, 5052-H32 supports forming and corrosion resistance, and A356-T6 suits complex cast structures.

For a broader material comparison, see Steel vs Aluminum. You can also review the CNC machining materials guide and aluminum CNC machining services.

FAQ

What is the yield strength of aluminum?

There is no single value. It depends on alloy, temper, product form, and material standard.

What is the yield strength of 6061-T6 aluminum?

A typical value is about 276 MPa, but the final design value should be confirmed for the specific product form and standard.

Which common aluminum alloy has the highest yield strength?

7075-T6 is generally one of the highest-strength common wrought aluminum choices, but corrosion, machinability, cost, and environment still matter.

Does heat treatment increase aluminum yield strength?

For heat-treatable alloys such as 6061 and 7075, solution treatment and aging can significantly increase yield strength.

MATSON METAL can evaluate the alloy, temper, manufacturing route, and finishing requirements for your aluminum part. Send your drawing, loads, tolerances, quantity, and application conditions for a manufacturing assessment.

Leave a Reply